K2O 9.1%, Na2O 7%, Al2O3 24.9%, SiO2 56% More fusible than feldspar, it has lower silica and higher soda and potassium levels and so can be used a lower melting temperatures. Important for use in vitreous bodies.
Glass jar is for illustration purposes only.